Bonded Neodymium magnets are produced using moulding techniques in simple tools & can be quickly machined into complex shapes. The material is isotropic offering approximately 10 MGO, or 30% of the energy seen in the sintered fully dense material.
It has a maximum operating temperature of 120°C and a rather poor temperature coefficient; the Curie temperature is 340°C. Due to its high Iron content these magnets are prone to corrosion and care is needed to avoid moisture or hostile environments.
Magnetic Properties of compression molding bonded NdFeB Magnets:
Grade
|
BNP-6
|
BNP-8
|
BNP-10
|
BNP-12
|
BNP-8H
|
Br (T)
|
0.52-0.60
|
0.60-0.65
|
0.65-0.70
|
0.70-0.76
|
0.55-0.62
|
HcB
|
KA/M
|
304-360
|
360-440
|
360-464
|
424-480
|
400-480
|
KOe
|
3.8-4.5
|
4.5-5.5
|
4.5-5.8
|
5.3-6.0
|
5.0-6.0
|
HcJ
|
KJ/m3
|
640-800
|
640-960
|
650-960
|
650-880
|
960-1280
|
KOe
|
8.0-10
|
8.0-12
|
8.0-12
|
8.0-11
|
12-16
|
(BH)Max
|
KJ/m3
|
40-56
|
56-72
|
72-80
|
80-96
|
48-72
|
MGOe
|
5-7
|
7-9
|
9-10
|
10-12
|
6-9
|
Density (g/cm3)
|
5.3-5.8
|
5.6-6.0
|
5.8-6.1
|
6.0-6.2
|
5.6-6.0
|
a Br (%/℃)
|
-0.13
|
-0.13
|
-0.07- -0.105
|
-0.13
|
-0.07- -0.13
|
Tw (℃)
|
140
|
140
|
120
|
130
|
130
|
|