Detailed Product Description
USE:
A213 : Seamless Ferritic and Austenitic Alloy-Steel Boiler,Superheater and Heat-Exchanger Tubes
|
Weight Count:(just for Alloy Steel)
Weight(Kg/M)=(OD-WT)*WT*0.02466
OD:Outside Diameter
WT:Wall-Thickness
|
A213 Alloy Boiler Tube Chemical Requirements
|
C max
|
Mn max
|
P max
|
S max
|
Si min
|
Cr max
|
Ni max
|
Mo max
|
Cu Max
|
T5
|
0.15
|
0.3-0.6
|
0.025
|
0.025
|
0.5
|
4.0-6.0
|
|
0.45-0.65
|
|
T11
|
0.05-0.15
|
0.3-0.6
|
0.025
|
0.025
|
0.5-1.0
|
1.0-1.5
|
|
0.44-0.65
|
|
T12
|
0.05-0.15
|
0.3-0.61
|
0.025
|
0.025
|
0.50
|
0.8-1.25
|
|
0.44-0.65
|
|
T22
|
0.05-0.15
|
0.3-0.6
|
0.025
|
0.025
|
0.5-1.0
|
1.9-2.6
|
|
0.87-1.13
|
|
T91
|
|
|
|
|
|
|
|
|
|
|
A213 Alloy Boiler Tube Mechanical Test
|
Tensile(Mpa)
|
Yeild(Mpa)
|
Elongation(%)
|
Hardness MAX
|
T5
|
415
|
205
|
30
|
89HRB
|
T11
|
...
|
...
|
...
|
...
|
T12
|
415
|
220
|
30
|
85HRB
|
T22
|
...
|
...
|
...
|
...
|
|
A213 Seamless Alloy Steel Boiler Tube Delivery Condition :
As different requirements,It including pickling,etc. AS per Standard
Packing:
1.Standard Packing
2.Woodbox Packing
Other Test:
1.Hydrostatic or Nondestructive Electric Test
2.Heat Treatment: according to Standard
3.Surface Condition:According to Standard.
4.Grain Size:According to standard
5.Sampling:flattening,flaring,grain size,Marking
|
|