Detailed Product Description
Iron-based amorphous ribbon:
Production speciation:
Thickness 0.02mm to 0.03mm,width 2.5mm to 170 mm. Customized size is also available upon requests.
Physical properties:
Saturate Induction |
1.56T |
Hardness(Hv) |
960kg/mm2 |
Curie Temperature |
410 degress C |
Density |
7.18g/cm3 |
Crystallization Temperature |
535 degress C |
Resistivity |
130μΩ-cm |
Saturate Magnetostriction |
27×10-6 |
|
|
Magnetic properties:
Product type
|
Transverse field annealed
|
No field annealed
|
Longitudinal field annealed
|
Maximum permeability |
>2×104 |
>20×104 |
>25×104 |
Saturate induction |
1.5T |
1.5T |
1.5T |
Remanence |
<0.5T |
01.0T |
1.2T |
Coercivity |
<4 A/m |
<2.4 A/m |
<4 A/m |
Core loss (50kHz, 1.4T) |
<0.2 W/kg |
<0.13 W/kg |
<0.3 W/kg |
Core loss (400kHz, 1.2T) |
<1.8 W/kg |
<1.25 W/kg |
<2 W/kg |
Core loss (8kHz, 1.0T) |
<80 W/kg |
<60 W/kg |
<100 W/KG |
Curves:


|